Effect of withdrawal rate transition on microstructural features of a single crystal Ni-based superalloy
F. Sadeghi, A. Kermanpur, D. Heydari, M. Bahmani; "Effect of withdrawal rate transition on microstructural features of a single crystal Ni-based superalloy", Cryst. Res. Technol., 2017, 52, 1700012.